Hello All,

Our EM lab melted a block meant for IHC staining and put it into plastic. Is there any way to get the tissue back to paraffin?

I know it's a long shot but just wondering....

Kenneth G Metzger HTL(ASCP)
Histology Supervisor
ARUP Labs
Salt Lake City, Utah
Phone: (801)583-2787 ext. 3101
Fax: (801) 584-5244
Email: kenneth.metzger at aruplab.com<mailto:kenneth.metzger at aruplab.com>


 -------------------------------------------------------------------
The information transmitted by this e-mail and any included
attachments are from ARUP Laboratories and are intended only for the
recipient. The information contained in this message is confidential
and may constitute inside or non-public information under
international, federal, or state securities laws, or protected health
information and is intended only for the use of the recipient.
Unauthorized forwarding, printing, copying, distributing, or use of
such information is strictly prohibited and may be unlawful. If you
are not the intended recipient, please promptly delete this e-mail
and notify the sender of the delivery error or you may call ARUP
Laboratories Compliance Hot Line in Salt Lake City, Utah USA at (+1
(800) 522-2787 ext. 2100


More information about the Histonet mailing list