[Histonet] Paraffin Blocks Cracking

Vanessa Avalos vavalos <@t> allergydermatology.com
Wed Jan 4 12:33:33 CST 2012


I have also noticed that the temperature in the lab makes a big difference. Now that it is colder outside and some heaters kick on check your temps. 

-----Original Message-----
From: histonet-bounces <@t> lists.utsouthwestern.edu [mailto:histonet-bounces <@t> lists.utsouthwestern.edu] On Behalf Of Brian foster
Sent: Wednesday, January 04, 2012 10:34 AM
To: histonet <@t> lists.utsouthwestern.edu
Subject: [Histonet] Paraffin Blocks Cracking

Hello all,


 I am studying for my HTL and have a question that has been a problem for me and was wondering if anyione out there can help. "What cuases paraffin blocks to crack ?" So far i have come up with it has to do the crystal formation during cooling, and I have seen some Histonet articles that say the block cooling plate at the embedding may be too cold ( less than -5 C). Can anyone confirm that is the is the correct cause of the problem?
_______________________________________________
Histonet mailing list
Histonet <@t> lists.utsouthwestern.edu
http://lists.utsouthwestern.edu/mailman/listinfo/histonet



More information about the Histonet mailing list