Mike
We place all of our bone sections on a hot plate (around 40 degrees C,
the paraffin should not melt) overnight and then stain them. If you
need to take a look at some images you can go to our web page, there
should be some images in the gallery on mouse joints, and a few pdf
files that you could down load that might be helpful.
Liz
Elizabeth A. Chlipala, BS, HTL(ASCP)
Premier Histology Laboratory, LLC
P.O. Box 18592
Boulder, Colorado 80308
Office: (303) 735-5001
Fax: (303) 735-3540
lizchlipala <@t> premierhistology.com
www.premierhistology.com
Ship to Address:
Premier Histology Laboratory
University of Colorado
MCBD, Room A3B40
Boulder, Colorado 80309
_________________________________
This email and any files transmitted with it may contain PRIVILEGED or
CONFIDENTIAL information and may be read or used only by the intended
recipient. If you are not the intended recipient of the email or any of
its attachments, please be advised that you have received this email in
error and that any use, dissemination, distribution, forwarding,
printing, or copying of this email or any attached files is strictly
prohibited. If you have received this email in error, please immediately
purge it and all attachments and notify the sender by reply email or
contact the sender at the number listed above if one is provided.
-----Original Message-----
From: histonet-bounces <@t> lists.utsouthwestern.edu
[mailto:histonet-bounces <@t> lists.utsouthwestern.edu] On Behalf Of Mike
Sohaskey
Sent: Wednesday, January 14, 2004 11:37 AM
To: histonet <@t> lists.utsouthwestern.edu
Subject: [Histonet] folds forming in bone/cartilage sections
Hello,
I find that, when sectioning EDTA-decalcified mouse tibiae at
5 - 10 microns, that folds (i.e., creases) frequently form
specifically within the growth plate cartilage as the sections dry
and adhere to the Superfrost slides. I have had no success with
increasing the amount of time that I float the sections on a water
bath prior to drying them on slides. I'm hoping that someone might
be able to offer a suggestion as to how I can overcome this
difficulty. Thanks very much.
MIKE
Michael Sohaskey, Ph.D.
University of California, Berkeley
Molecular and Cell Biology
585 Life Sciences Addition
Berkeley, CA 94720-3200
sohaskey <@t> socrates.berkeley.edu
(510) 643-2775 (phone)
_______________________________________________
Histonet mailing list
Histonet <@t> lists.utsouthwestern.edu
http://lists.utsouthwestern.edu/mailman/listinfo/histonet
More information about the Histonet
mailing list