<DIV>We had this same problem.&nbsp; We had control over everything, too. We stopped using Sta-On, etrc.&nbsp; ANd we still had the problem&nbsp; - haziness, it looked like the mucin was staining, but we also had the fuzziness on non-GI's as well.&nbsp; It turned out to be two things--the hematoxylin we were using and the timing of it and the temperature of the water on the stainer--it was too cold.</DIV></BODY></HTML>