Hi all,
We are using Parapast X-tra on the Peloris at 65C (factory default), and I am thinking this is just way too hot (X-tra has a melting point of 52C). Leica of course will not commit to an opinion. Is anyone else using paraplast x-tra on their Peloris?
Thank you,
Noëlle
Noëlle Linke, MS, HTL(ASCP) QIHC
Manager, Anatomic Pathology
Pacific Diagnostic Laboratories
nlinke at sbch.org<mailto:nlinke at sbch.org>
Phone: (805) 324-9814
Fax: (805) 696-6433
________________________________
CH Disclaimer: This electronic mail message is intended exclusively for the individual or entity to which it is addressed. This message, together with any attachment, may contain confidential and privileged information. Any views, opinions or conclusions expressed in this message are those of the individual sender and do not necessarily reflect the views of Cottage Health, its subsidiaries or affiliates. This document may also contain information covered under the Health Insurance Portability and Accountability Act (HIPAA, PL 104-191) and implementing regulations and must be protected in accordance with those provisions. Re-disclosure without patient consent or as otherwise permitted by law is prohibited. Any unauthorized review, retransmission, use, printing, copying, retention, disclosure, distribution or the taking of any action in reliance upon this information by persons or entities other than the intended recipient is strictly prohibited and may be unlawful. If you have received this message in error, please immediately advise the sender by reply email message to the sender and delete all copies of this message from your system without copying.
________________________________
More information about the Histonet
mailing list