[Histonet] formic acid decal
    Elizabeth Chlipala 
    liz <@t> premierlab.com
       
    Fri Jun 17 10:17:28 CDT 2005
    
    
  
Trisha
I have used 20% formic acid made up in distilled water on sheep tibias
and it worked just fine.
Liz
Elizabeth A. Chlipala, BS, HTL(ASCP)QIHC
Manager
Premier Laboratory, LLC
P.O. Box 18592
Boulder, Colorado 80308
Office: (303) 735-5001
Fax: (303) 735-3540
liz <@t> premierlab.com
www.premierlab.com
 
Ship to Address:
Premier Laboratory
University of Colorado
MCDB, Room A3B40
Boulder, Colorado 80309
-----Original Message-----
From: histonet-bounces <@t> lists.utsouthwestern.edu
[mailto:histonet-bounces <@t> lists.utsouthwestern.edu] On Behalf Of Trisha
Emry
Sent: Thursday, June 16, 2005 2:54 PM
To: histo
Subject: [Histonet] formic acid decal
I need to speed up the decal process on some large bone samples.
What is the highest precentage of formic acid that I can use without
damaging the bones?
I am using sodium formate with formic acid now.
Thanks,
Trisha
Seattle
_______________________________________________
Histonet mailing list
Histonet <@t> lists.utsouthwestern.edu
http://lists.utsouthwestern.edu/mailman/listinfo/histonet
    
    
More information about the Histonet
mailing list